Attention!
Next, put a grid-wrap on crushed stone and pressed it with metal pins. This is necessary so that the concrete site does not fall apart and does not crack. After pour the site with a previously prepared solution or concrete. Attention! When pouring, the terraces leave a thin strip of 3-5 cm along the edges of the site, since concrete under different climatic conditions has the ability to narrow and expand, which leads to the destruction of concrete. If the filling of the site occurs when it is hot on the street, it must be periodically watered with cold water, so the upper layer will not crack. And if the site is poured in cold weather, then it must be isolated from the cold — covered with a film. Since the moisture in the solution does not completely dry and freeze, the concrete will subsequently crumble. Observing all the rules, you will see the quality of the concrete site.