With a solvent until
The technology of the use of OZK-45 and OZK-45D to obtain a sustainable coating involves a mixture of the base with a hardener (they are delivered both wholesale and retail in separate packages) with subsequent exposure at an air temperature of 20 degrees for 1 hour. In the future, the composition can be mixed with a solvent until the desired level of viscosity is obtained and used for the preparation of an alkaline -resistant enamel or film that has a significant electrical resistance.